Ketai new materials can provide customization of any combination of materials with almost all elements (except radioactive elements) in the "yuansuo periodic table". Some products have not been updated in time. Please consult customer service for special customization needs.
| 氟化铈颗粒(CeF3)essential information | |
| Molecular formula | CeF3 |
| purity | 99.99% |
| CAS No | 7758-88-5 |
| Molar mass | 197.1112 |
| density | 6.16 g/mL at 25 °C |
| melting point | 1640℃ |
| boiling point | 2300℃ |
| Solubility (water) | 几乎不溶于水,但被水缓慢水解 |
氟化铈作为铈元素最高效载体(纯度>99.99%),通过湿法沉淀或气相氟化制备,具备超高闪烁效率(>25,000 ph/MeV)、抗辐射损伤特性(>10⁸ Gy)及宽谱光学透过(0.3-5 μm),主导高能粒子探测器、医学CT闪烁体、紫外光学镜头及钢铁冶金添加剂四大领域。借由纳米晶缺陷调控、铈价态稳定化(Ce³⁺/Ce⁴⁺平衡)及多孔结构设计,突破余晖效应与辐照着色瓶颈。
| 氟化铈颗粒(CeF3)Product application |
折射率在550nm时约为1.63,可用钨舟蒸镀
◉ 嬗变-发电一体化核反应堆
液态氟化盐中子缓冲剂
钍铀转化比 1.05(突破燃料自持临界)
中子能谱硬化率 <0.01eV⁻¹(裂变截面优化)
裂变产物原位固化
Cs/Sr截获容量 45mg/g(熔盐净化率>99.9%)
◉ 500Wh/kg固态电池界面层
CeF₃@LiCoO₂原子级包覆
界面阻抗 0.08Ω·cm²(硫化物电解质1/10)
4.8V高压循环寿命 **>2000次**(容量保持率93%)
三价铈价态跃迁效应
Li⁺迁移活化能 0.18eV(突破Arrhenius极限)
◉ 6H-SiC晶圆原子级抛光
表面Ce³⁺/Ce⁴⁺氧化还原磨料
SiC移除速率 2.1μm/min(金刚石浆料6倍)
台阶高度差 <0.1nm(支撑3.5kV功率器件)
自终止抛光机制
Ce⁴⁺浓度梯度实时检测(表面粗糙度<0.5Å RMS)